RTU Research Information System
Latviešu English

Publikācija: Effect of Thermal Treatment on Thermoelectric Properties of Extruded TiO2 Ceramics

Publication Type Scientific article indexed in SCOPUS or WOS database
Funding for basic activity Unknown
Defending: ,
Publication language English (en)
Title in original language Effect of Thermal Treatment on Thermoelectric Properties of Extruded TiO2 Ceramics
Field of research 2. Engineering and technology
Sub-field of research 2.5 Materials engineering
Authors Agnese Pūra
Jānis Ločs
Līga Bērziņa-Cimdiņa
Keywords Extrusion; Thermoelectric properties; Titanium dioxide
Abstract TiO2 samples were obtained by extrusion process, sintered in air at 1000 °C, 1100 °C, 1200°C and 1300 °C and, afterwards, thermally treated under vacuum conditions at 1250 °C for 1 hour applying two different heating/cooling rates (2 °C/min and 5 °C/min). It was found that thermal treatment conditions substantially affected thermoelectric properties of the samples. Increasing sintering temperature, during the sample thermal treatment in air, the electrical conductivity of the specimens increased, while Seebeck coefficient decreased. With an increase in the heating rate during the vacuum heat treatment of the samples, the electrical conductivity of the samples decreased, while Seebeck coefficient increased.