For understanding of reasons of glass fiber breakage comprehensive investigation of defected areas was carried out and the glass chemical composition and properties were compared. Visual evalution of breaking spots showed that there are at least two types of glass fiber breakage - extraneous crystalline inclusions and breaking spot without any visual changes. In the place of defects origin, EDAX analyses showed the difference in distribution of chemical elements in bulk and on the glass surface


Keywords
glass fibre, quality, defect, filament breakage

Sētiņa, J., Akišins, V., Pētersone, L., Veseris, V., Juhņeviča, I. Influence of Various Factors on the Glass Fibre Breakage Rate. In: BaltSilica 2011 : Book of Abstracts of the 5th Baltic Conference on Silicate Materials, Latvia, Riga, 23-25 May, 2011. Riga: RTU Publishing House, 2011, pp.86-87. ISSN 2243-6057.

Publication language
English (en)
The Scientific Library of the Riga Technical University.
E-mail: uzzinas@rtu.lv; Phone: +371 28399196