Production of ZnO AND CdO-ZnO Thin Films by Extraction–Pyrolytic Method
A. Cvetkovs, O. Kiselova, U. Rogulis, Vera Serga, R. Ignatans

The extraction-pyrolytic method has been applied to produce the ZnO and CdO-ZnO thin films on glass and quartz glass substrates. According to X-ray diffraction measurements, the ZnO and CdO phases have been produced with an average size of crystallites about 8–42 nm in the films. The thickness of the layers measured by a profilometer has been up to150 nm. The surface morphology measurements show that the surface of the films may be rough and non-continuous. The SEM results confirm the dependence between the preparation procedure and the quality of the thin film.


Pieteikuma datums
27.07.2016.
Atslēgas vārdi
CdO-ZnO thin films, extraction-pyrolytic method, surface morphology, X-ray diffraction.
DOI
10.1515/lpts-2016-0021
Hipersaite
http://www.degruyter.com/view/j/lpts.2016.53.issue-3/issue-files/lpts.2016.53.issue-3.xml
Zinātniskās darbības koordinācijas un informācijas nodaļa.
E-pasts: elza.vecpuise@rtu.lv; Tālr: +371 26013889