Influence of Various Factors on the Glass Fibre Breakage Rate
            
            BaltSilica 2011 : Book of Abstracts of the 5th Baltic Conference on Silicate Materials
            2011
            
        
                Janīna Sētiņa,
        
                Vasīlijs Akišins,
        
                Laila Pētersone,
        
                Valdis Veseris,
        
                Inna Juhņeviča
        
    
            
            
            For understanding of reasons of glass fiber breakage comprehensive investigation of defected areas was carried out and the glass chemical composition and properties were compared. Visual evalution of breaking spots showed that there are at least two types of glass fiber breakage - extraneous crystalline inclusions and breaking spot without any visual changes. In the place of defects origin, EDAX analyses showed the difference in distribution of chemical elements in bulk and on the glass surface
            
            
            
                Atslēgas vārdi
                glass fibre, quality, defect, filament breakage
            
            
            
            
            Sētiņa, J., Akišins, V., Pētersone, L., Veseris, V., Juhņeviča, I. Influence of Various Factors on the Glass Fibre Breakage Rate. No: BaltSilica 2011 : Book of Abstracts of the 5th Baltic Conference on Silicate Materials, Latvija, Riga, 23.-25. maijs, 2011. Riga: RTU Publishing House, 2011, 86.-87.lpp. ISSN 2243-6057.
            
                Publikācijas valoda
                English (en)